A sealing engineer is reviewing a flange gasket that failed in a steam service. The gasket is made from unfilled PTFE. It has cold-flowed out of the flange gap, and the bolt load has dropped. The engineer replaces it with a graphite-filled grade of Modified PTFE Sheets. The new gasket holds the bolt load, and the joint does not leak. The engineer asks why a small amount of graphite makes such a large difference. The answer is in the way the graphite particles interrupt the polymer chain movement and conduct heat away from the sealing surface. This guide explains how graphite improves the performance of filled PTFE sheets and how to specify the correct grade.
Unfilled PTFE has excellent chemical resistance and a very low friction coefficient, but it has two weaknesses in sealing service. The first is cold flow, also called creep. Under a sustained compressive load, the polymer chains slide past each other, and the material deforms permanently. The gasket becomes thinner, the bolt load drops, and the joint leaks. The second is poor thermal conductivity. The heat generated at the sealing surface cannot escape, and the local temperature rises, which accelerates the creep and the wear. In our factory, we compound Modified PTFE Sheets with fillers to address both weaknesses. Taifno has been manufacturing filled PTFE products for over 12 years.
The cold flow is not a defect. It is a property of the polymer. The solution is not to change the polymer but to add a filler that restricts the chain movement. Graphite is one of the most effective fillers for this purpose because it is chemically inert, thermally conductive, and available in a range of particle sizes and purities.
Graphite is added to the PTFE resin at a loading of 5 to 25 percent by weight, depending on the application. The graphite particles are dispersed through the polymer matrix. When the material is compressed, the particles act as physical obstacles that prevent the polymer chains from sliding. The result is a lower creep rate and a higher retention of bolt load. The table below compares the creep behavior of unfilled and graphite-filled grades.
| Grade | Graphite loading | Compression creep after 100 h at 10 MPa, 100°C | Bolt load retention |
| Unfilled PTFE | 0% | 18 to 25% | Low |
| Graphite filled 5% | 5% | 10 to 14% | Moderate |
| Graphite filled 15% | 15% | 5 to 8% | High |
| Graphite filled 25% | 25% | 3 to 6% | Very high |
In our factory, we test the creep resistance of every graphite-filled batch according to ASTM D621 or an equivalent method. The test measures the reduction in thickness under a constant load at a controlled temperature. The result is recorded on the certificate of analysis. Ningbo Taifno PTFE Plastic Products Co., Ltd. provides the creep data with each order so that the gasket designer can verify the bolt load retention.
PTFE has a thermal conductivity of about 0.25 watts per meter kelvin, which is low compared with metals. Graphite has a thermal conductivity of 100 to 400 watts per meter kelvin, depending on the crystal orientation and the purity. When graphite is dispersed in the PTFE matrix, it forms a conductive network that carries heat away from the sealing surface. The higher thermal conductivity reduces the local temperature at the gasket face, which reduces the creep rate and extends the service life. The table below shows the thermal conductivity of different filled grades.
| Grade | Filler system | Thermal conductivity (W/mK) | Continuous service temperature |
| Unfilled PTFE | None | 0.25 | 260°C |
| Graphite filled 15% | Graphite | 0.45 to 0.55 | 260°C |
| Graphite + carbon 25% | Graphite and carbon | 0.60 to 0.80 | 280°C |
| Graphite + glass 20% | Graphite and glass fiber | 0.50 to 0.65 | 260°C |
Sealing engineer's note: The thermal conductivity is not the only factor. The contact resistance between the gasket and the flange also matters. A gasket that is rough or that has a low compression will have a high contact resistance, and the heat will not flow into the flange even if the gasket conductivity is high. In our factory, we recommend a surface finish of Ra 0.4 to 0.8 micrometers on the sealing face and a compression of 25 to 35 percent for the graphite-filled grade. Ningbo Taifno PTFE Plastic Products Co., Ltd. provides the recommended compression and surface finish with each grade.
Graphite is a solid lubricant. Its layered crystal structure allows the layers to slide over each other with low friction. When graphite is added to PTFE, the friction coefficient is not dramatically reduced, because PTFE is already a low friction material. But the wear rate is reduced, especially in dry running and in high pressure applications. The graphite particles form a transfer film on the mating surface, and this film protects the PTFE from abrasive wear. The wear rate of a graphite-filled grade is typically 10 to 100 times lower than the unfilled grade under the same conditions. In our factory, we measure the wear rate on a pin on disc tester and report the result as a volume loss per unit load and distance. Ningbo Taifno PTFE Plastic Products Co., Ltd. can provide the wear data for each grade and each mating surface material.
The friction and wear behavior also depends on the counterface. A graphite-filled PTFE running against a smooth stainless steel surface will form a stable transfer film. Running against a rough or a corroded surface will not form the film, and the wear rate will be higher. We recommend a counterface surface finish of Ra 0.2 to 0.4 micrometers and a hardness of at least 200 HB for the best wear performance.
The specification should include the graphite loading, the particle size, the purity, the sheet thickness, the surface finish, and the compression requirement. The buyer should also specify the test method for the creep resistance and the thermal conductivity. The verification should include the material certificate, the creep test report, the thermal conductivity measurement, and the dimensional inspection. In our factory, we provide all four documents with each batch. We also keep a sample of the compound for each batch so that the filler content can be traced if a question arises later. Ningbo Taifno PTFE Plastic Products Co., Ltd. can arrange a third party test if the buyer requires it.
We recommend that the buyer specify the graphite loading by weight and not just the grade name. A grade that is described as "graphite filled" may contain 5 percent or 25 percent graphite, and the difference in creep resistance is significant. The buyer should ask for the actual loading and the corresponding creep data before approving the grade.
Graphite improves the performance of filled PTFE sheets by restricting the creep, by increasing the thermal conductivity, and by reducing the wear rate. The graphite loading determines the degree of improvement, and the particle size determines the surface finish and the sealing performance. The buyer should specify the loading, the particle size, and the test method, and should verify the creep, the thermal conductivity, and the wear data before approving the grade. When the grade is selected correctly, the graphite filled sheet provides a longer service life than the unfilled sheet in high pressure and high temperature sealing applications.